What is a Hammer mill crusher?

Hammer crusher is a device for crushing materials in the form of impact. It can crush materials with a maximum particle size of 600-1800 mm to 25 mm or smaller. Hammer crusher is suitable for crushing medium-hard materials such as limestone, slag, coke, coal and other materials in cement, chemical, electric power, metallurgical and other industries.

What are the types of hammer crushers

Zoneding mainly provides 3 types of hammer crushers: hammer crushers, heavy type hammer crushers, mobile hammer crusher, etc. Here are details of these 3 types of hammer crushers.

Diesel Hammer Crusher
Diesel Hammer Crusher
Diesel Hammer Crusher
Diesel Hammer Crusher
Heavy hammer crusher
Mobile heavy hammer crusher

What is the structure of a hammer crusher

A hammer mill crusher is mainly composed of the frame, rotor, hammer head, main shaft, and other components.

Hammer crusher structure
Hammer crusher structure

Heavy hammer crusher structure
Heavy hammer crusher structure
Hammer crusher important parts

The working principle of the hammer mill

The working principle of the hammer mill is to crush materials by the impact force of the high-speed rotating hammer head.

When working, the motor drives the rotor to rotate at a high speed, and the materials are evenly sent into the crushing cavity. The high-speed rotating hammer heads impact and crush the minerals. The crushed materials rush to the impact plate and grate bar at high speed. At the same time, the materials impact each other and are crushed many times.

Hammer Crusher Production Line Flowchart

Parameter

PC Hammer Crusher
PCZ Heavy Hammer Crusher

PC Hammer Crusher

Specification Capacity(t/h) Power (kw)
PC 400×300 3-10 4P 11
PC 600×400 6-22 4P 22
PC 800×600 10-40 4P 55
PC 1000×800 15-50 4P 75
PC 1000×1000 18-75 4P 90
PC 1200×1200 22-95 4P 132

PCZ Heavy Hammer Crusher

Model Rotor diameter×length (mm) Feed Opening Length×width(mm) Feeding Size (mm) Processing Capacity(t/h) Power (kw) Dimensions L×W×H (mm)
PCZ1308 Φ1330×790 870×780 ≤380 60-160 132 2880×2130×2390
PCZ1410 Φ1400×1000 1060×740 ≤450 80-210 2×90(160) 2830×2100×2485
PCZ1610 Φ1600×1000 1090×930 ≤480 100-230 2×132 3370×2415×2750
PCZ1612 Φ1600×1200 1340×1140 ≤500 120-350 2×160 3370×2613×2750
PCZ1615 Φ1600×1500 1570×1140 ≤550 200-550 2×200 3370×2925×2750
PCZ1716 Φ1700×1600 1420×1200 ≤600 400-850 2×250 3520×3000×3210
PCZ1720 Φ1700×2000 2030×1200 ≤650 500-1000 2×400 3670×3390×3330
PCZ1920 Φ1900×2000 1980×1210 ≤750 800-1500 2×500 4490×3910×3600
PCZ2225 Φ2200×2500 2530×1610 ≤1000 1500-3000 1250 4890×5010×4560

Customer Site

Hammer crusher site

FAQ

Q1. Who are we?
A1: Zoneding Machine is manufacture of mining machine which is located in Henan province of China. We have been professional on grinding mill, stone crushers, sand making machines, production line for ore beneficiation, sand and aggregate industries since 2004.

Q2. What is our main crusher products?
A2: Jaw Crusher/Cone Crusher/Vibrating Screen/Sand Making Machine/Mobile Stone Crusher Plant/Vibrating Feeder/Fine Sand Recovery Machine/Screw Sand Washing Machine/Impact Crusher/Vertical Shaft Impact Crusher/Hammer Crusher/Belt Conveyor/Stone Crushing Plant.

Q3. What about the price ?
A3: We are able to give you competitive price than market one cuz we are factory, and we have a policy that ” for saving time and absolutely honest” business attitude,we quote as low as possible for any customer, and discount can be given according to quantity

Q4. What services can we provide?
A4: Accepted Delivery Terms: FOB, CFR, CIF;
Accepted Payment Currency: USD,EUR, CNY;
Accepted Payment Type: T/T,L/C;
Language Spoken: English,Chinese,Spanish,Arabic,French,Russian

Q5: When will the delivery be?
A5: For inventory goods, we can ship them within 3-5 days. For customized equipment and other devices, we will specify according to clients’ needs as we quote.

loading…

已经是到最后一篇内容了!

We use cookies to ensure that we give you the best experience on our website. If you continue to use this site we will assume that you are happy with it.
Privacy Policy

OK
Open chat
1
Scan the code
Hello 👋
Can we help you?