            The molecular formula of hematite is Fe2O3; it belongs to weak magnetite iron ore content. It usually accretes with magnetite ore. In China, hematite as a major mineral in quite a number of iron ore. The main origins of iron ore are Australia, Brazil, India, Canada, Russia, etc.

            The density of hematite is 4.8-5.3t/m³, hardness is 5.5-6.5, loose density is 2.5-3.0t/m³.

            The crushing system of hematite ore uses Three sections + One closed circuit process generally.

            After hematite ore crushed, its basic beneficiation process is Periodicity grinding or continuous grinding—weak Magnetic Separator—high gradient strong Magnetic Separator—anion reverse Flotation process. According to the difference of undressing ore grade, embedded cloth degree, gangue minerals composition and undressing ore properties, it can be used Degree Separator. Re-election for coarse grain. If S, P elements are exceeded bit, the Flotation process should be added to impurity. a trial should be made to improve the reliability of beneficiation process.

            The main equipments include Jaw Crusher, Cone Crusher, Circular Vibrating Screen, Ball Mill, Spiral Classifier, hydrocyclone or High Frequency Fine Screen, Magnetic Separator, Flotation Machine, Thickener, Filter, Spiral Chute etc. Zoneding Machine has a great experience of this magnetite beneficiation process. We can form varieties of specifications of crushing, screening, grinding and provide varieties of beneficiation equipments.

            After beneficiated, the grade of iron concentrate is up to 64% or more, SiO2 amount should be controlled under 6% ( as low as better), the amount of toxic elements like S, P should be achieved the standards of national and iron enterprise.

            The basic process of magnetite beneficiation as follows:

            The typical case of magnetite beneficiation is concentrator of Qidashan Anshan in Liaoning Province, concentrator of Donganshan in Anshan in Liaoning province; concentrator of Xijiaying in Hebei province, etc.


     

    Order Online

    If you have some questions about our products, please feel free to fill out the form below, and we will contact you within 24 hours. Rest assured that we won’t reveal your information to anyone.

    Your Name: *
    Email: *
    Country:
    Tel.:
    Product:
    Please enter detailed information in the form below, such as raw materials, capacity(t/h,t/d), materials feeding size(mm), finial products size(mm) or other requirements.
    Message: *
     
    ABOUT US
    About Zoneding
    Zoneding Certifications
    Zoneding FAQ
    Zoneding Cases
    Zongding Service
    PRODUCTS
    Crushing & Screening Equipment
    Beneficiation Equipment
    Mobile Crushing Plant
    Grinding Plant
    Drying Equipment
    SOLUTIONS
    Different Materials Crushing Line
    Different Capacities Crushing Line
    Minerals Beneficiation Plant
    CONNECT WITH US
    LinkedIn® Find, connect, and collaborate. ---- Join Us
    Twitter® Instant updates about what's going on. ---- Follow Us
    Facebook® Connect with old and new friends. ---- Let's Be Friends
    google+

    Copyright:2014 Zhengzhou Zhongding Heavy Duty Machine Manufacturing Co.,Ltd.