    Chromite Ore Processing

            Chromite is found in peridotite from the Earth's mantle. It also occurs in layered ultramafic intrusive rocks. In addition, it is found in metamorphic rocks such as some serpentinites. Ore deposits of chromite form as early magmatic differentiates. It is commonly associated with olivine, magnetite, serpentine, and corundum.

    Major components:
            (Fe, Mg)Cr2O4
    Mohs hardness:
            5.5
    Available machine:
            Jaw Crusher ,Ball Mill,Vibrating Screen
    Applications:
            Metallurgical,Refractory,Chemical
    Introduction of chrome ore beneficiation plant:
            Ore dressing means the production process in which the extracted ore goes through several procedures finally becomes the concentrate in accordance with the smelting requirements. Ore dressing flow mainly includes crushing by crusher, separating by vibrating screen, grinding by ball mill and classifying by classifier; the separation of minerals consists of weight, flotation, and electric separation, etc. Dehydration of minerals includes enrichment, filtration, drying, and other procedures. The equipment of mineral processing cover feeder, crusher, ball mill, classifier, vibrating screen, rocking bed, magnetic separator, mix tank, flotation machine and so on.
    Working principle of chrome ore beneficiation plant:
            The extracted ore should be crushed by jaw crusher initially. When it gets the reasonable fineness, it is transported into ball mill by elevating conveyer and feeder, and is milled by ball mill. The subtle milled ore gets the next procedure: classification. There is a theory that if the weights of solid particles are different, the sedimentations will be different, and the mixed ore can be classified by screw classifier. The classified ore gets into magnetic separator. Since the specific magnetization coefficients of ores are different, the magnetic substance of mixed ore is separated from others with magnetic and mechanical force. The mineral matter, which has been separated by magnetic separator initially, is transported into flotation machine by, and different medicines are added according to different characteristics of ore, so that the needed ore is separated from others. Since the separated ore are wet, they should be dewatered by thickner initially, and dried by drier. Finally, the dry minerals come into being.

    Order Online

    If you have some questions about our products, please feel free to fill out the form below, and we will contact you within 24 hours. Rest assured that we won’t reveal your information to anyone.

    Your Name: *
    Email: *
    Country:
    Tel.:
    Product:
    Please enter detailed information in the form below, such as raw materials, capacity(t/h,t/d), materials feeding size(mm), finial products size(mm) or other requirements.
    Message: *
     
    ABOUT US
    About Zoneding
    Zoneding Certifications
    Zoneding FAQ
    Zoneding Cases
    Zongding Service
    PRODUCTS
    Crushing & Screening Equipment
    Beneficiation Equipment
    Mobile Crushing Plant
    Grinding Plant
    Drying Equipment
    SOLUTIONS
    Different Materials Crushing Line
    Different Capacities Crushing Line
    Minerals Beneficiation Plant
    CONNECT WITH US
    LinkedIn® Find, connect, and collaborate. ---- Join Us
    Twitter® Instant updates about what's going on. ---- Follow Us
    Facebook® Connect with old and new friends. ---- Let's Be Friends
    google+

    Copyright:2014 Zhengzhou Zhongding Heavy Duty Machine Manufacturing Co.,Ltd.