    Calcite Processing

            Calcite powder is a natural form of calcium carbonate with extremely high whiteness, purity and free flowing in nature. Calcite powder and coated calcite powder has a pivotal role in the modern industrial like plastic, paint, cosmetic, paper, PVC pipe etc. due to its versatility, availability, and traceability.

    Major components:
            CaCO3
    Mohs hardness:
            3.0
    Available crusher:
            Cone Crusher,Jaw Crusher,Ball Mill
    Applications:
            Cement,Chemical, and refractory.

    Calcite Processing Plant:
            Big calcite materials are fed to the jaw crusher evenly and gradually by vibrating feeder through a hopper for primary crushing. After first crush, the material will transferred to impact crusher by belt conveyor for secondary crush; the crushed calcite materials will then transferred to vibrating screen for separating. After separating, the parts that can meet standard will be transferred away as final products, while the other parts will be returned to impact crusher, thus forming a closed circuit. Size of final products can be combined and graded according to your specific requirement.

    Calcite Grinding Process:
            Ball Mill is the key machine in calcite grinder plant. Ball mill can be used to grind various ores and other materials and has found its extensive application in the field of mine-selection, building materials and chemicals. And the ball mill can also be divided into two kinds: the dry process and wet process. And according to the different mine discharging types, the ball mill can also be divided into two kinds: grid type and over-flow.
            We manufacture and install complete line for obtaining micronised Calcite (CaCO3) from 75 micron till 1 micron according to the request of the customer. Our system is based on dry grinding and classification of particles.
     

    Calcite processing plant

    1)Raw material stock Bunker
    2) Conveyor Band
    3) Hummer Crusher
    4) Elevator
    5) Feeding Bunker
    6) Seperator
    7) Rotary Valve
    8) Ball Mill
    9) Jet plus Filter
    10) Packing Machine
    11) Radial Fan
    12) Screw Conveyor
    13) Electrical Control Board

    Calcite Processing Plant

    Order Online

    If you have some questions about our products, please feel free to fill out the form below, and we will contact you within 24 hours. Rest assured that we won’t reveal your information to anyone.

    Your Name: *
    Email: *
    Country:
    Tel.:
    Product:
    Please enter detailed information in the form below, such as raw materials, capacity(t/h,t/d), materials feeding size(mm), finial products size(mm) or other requirements.
    Message: *
     
    ABOUT US
    About Zoneding
    Zoneding Certifications
    Zoneding FAQ
    Zoneding Cases
    Zongding Service
    PRODUCTS
    Crushing & Screening Equipment
    Beneficiation Equipment
    Mobile Crushing Plant
    Grinding Plant
    Drying Equipment
    SOLUTIONS
    Different Materials Crushing Line
    Different Capacities Crushing Line
    Minerals Beneficiation Plant
    CONNECT WITH US
    LinkedIn® Find, connect, and collaborate. ---- Join Us
    Twitter® Instant updates about what's going on. ---- Follow Us
    Facebook® Connect with old and new friends. ---- Let's Be Friends
    google+

    Copyright:2014 Zhengzhou Zhongding Heavy Duty Machine Manufacturing Co.,Ltd.