    Compound Crusher

    【Feed Size】:50-100mm

    【Capacity】:5-100t/h

    【Application】:mining, metallurgy, refractory, cement, coal, glass, ceramics, and electric power industries.

    【Introduction】:Compound crusher is widely used in medium or fine crushing of hard or special hard materials as mining ore, cement, refractory, bauxite, carborundum, glass raw materials, etc. It is also widely used i

    WhatsApp: 18637198006

    Product Search

    Contact

    点击对话或留言

    Brief Introduction:

          This crusher is designed and optimized according to crushing technology at home and abroad, its performance has reached the advanced level, for crushing all kinds of hard ores, can be widely used in mining, metallurgy, refractory, cement , coal, glass, ceramics, and electric power industries. Compound crusher has big crushing ratio, the discharged size can be adjusted, not affected by the weariness of hammer board and the impact liner, Due to no screen bar setting, it can crush high moisture and mud materials, but not be clogged.
     
          Compound crusher, is widely used in stone crushing line or sand production line. This series crusher is suitable for crushing limestone, clinker, coal and other minerals of building materials, mining, metallurgy, chemical industry. its compressive strength is not more than 140 Mpa, humidity less than 15%.

    Features:

          Our compound crusher has large crushing ratio, higher yield, with 1.4 times yield than other crushers. It has efficient crushing capacity for shale, glass, ceramics, river gravel, granite, basalt, iron ore, bluestone, metal ores and other hard materials, particularly widely used in the mechanism aggregates and metal ores. Its wearing parts employ multi-alloy wear-resistant materials with high hardness, high toughness, life expectancy increased by 2-3 times; the gap between hammer and impact plate is adjustable, to meet the crushing requirements of variety materials.
          1.large crushing ratio, no screen bar, no clogging when crushing high moisture and mud materials.
          2. Bearings horizontal arrangement, long life, can crush high temperature materials (such as cement clinker).
          3. Adopt flexible adjustment mechanism, the non-crushing materials can be automatically discharged, will not damage the equipment.
          4. The rotor block is unique structure; the rotor block will not wear. The back cavity is with screw rod or hydraulic opening mechanism; you can easily replace wearing parts. not opening the equipment.

    Technical Parameters:

    Model
    800
    1000
    1250
    1500
    1750
    Rotater Diameter(mm)
    650
    800
    1000
    1250
    1560
    Cylinder Height(mm)
    800
    850
    850
    1000
    1410
    Rotating Speed(r/min)
    1350
    970
    740
    650
    600
    Input Size(mm)
    50
    70
    100
    100
    100
    Output Size (mm)
    0-5
    0-5
    0-5
    0-5
    0-5
    Capacity (t/h)
    5-15
    10-30
    20-60
    30-80
    40-100
    Motor
    Power(kw)
    30
    55
    75
    110
    132
    Rotating Speed
    1440
    1440
    750
    750
    750
    Overall Dimension(L×W×H)(mm)
    2200×860×1980
    2700×1160×2000
    2800×1400×2730
    3100×1900×2300
    3350×2100×2800
    Weight (t)
    2.3
    4.5
    9.73
    18.1
    26.61
     

    Related Cases:

    >>Learn more

    Order Online

    If you have some questions about our products, please feel free to fill out the form below, and we will contact you within 24 hours. Rest assured that we won’t reveal your information to anyone.

    Your Name: *
    Email: *
    Country:
    Tel.:
    Product:
    Please enter detailed information in the form below, such as raw materials, capacity(t/h,t/d), materials feeding size(mm), finial products size(mm) or other requirements.
    Message: *
     
    ABOUT US
    About Zoneding
    Zoneding Certifications
    Zoneding FAQ
    Zoneding Cases
    Zongding Service
    PRODUCTS
    Crushing & Screening Equipment
    Beneficiation Equipment
    Mobile Crushing Plant
    Grinding Plant
    Drying Equipment
    SOLUTIONS
    Different Materials Crushing Line
    Different Capacities Crushing Line
    Minerals Beneficiation Plant
    CONNECT WITH US
    LinkedIn® Find, connect, and collaborate. ---- Join Us
    Twitter® Instant updates about what's going on. ---- Follow Us
    Facebook® Connect with old and new friends. ---- Let's Be Friends
    google+

    Copyright:2014 Zhengzhou Zhongding Heavy Duty Machine Manufacturing Co.,Ltd.